search  current discussion  categories  glazes - cone 4-7 

more cone6 ox glazes- everybody please!!!

updated wed 27 sep 00

 

Earl Brunner on mon 25 sep 00


Patrick, there is not enough information here to know what
glaze you would be talking about. Sometimes when people
reply, the mail seems to form an automatic link to the
previous pot, but you don't even have that.

People, when responding to another post PLEASE provide
enough information to make the link, otherwise it seems a
waste. Perhaps the writer of the original message may make
the connection, but if they are the only ones then send it
directly to them and don't tie up the list. I came home from
work tonight and had 96 messages to go through.

patrick conrey wrote:
>
> Have you tried this glaze without the colorants???
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.

--
Earl Brunner
http://coyote.accessnv.com/bruec
mailto:bruec@anv.net

Sharon31 on tue 26 sep 00


There is another problem with a question like this!
Let us say, on Sunday for a request for ^6 glazes. I make a big list and
mail it, on Friday I see in Clayart a new letter "hi! does anyone can
share...." . So I would suggest to newcomers to the list, or these that on
Sunday did not pay attention Go to the archives!
I did it this time asked for ^6 glazes and got in this site
http://lsv.ceramics.org/scripts/wa.exe?S2=clayart&L=CLAYART&q=&s=%5E6+glazes
&f=&a=&b=
1824 matches (only the first 50 will be shown). of coarse you can ask for
more detailed subject, and if you want letters of misterbin@holywood.com,
add his name and you get all the letters he got on the subject you wanted.
After that ask again!

Ababi Sharon
sharon@shoval.org.il
http://www.milkywayceramics.com/cgallery/asharon.htm



----- Original Message -----
From: Earl Brunner
To:
Sent: Tuesday, September 26, 2000 06:37
Subject: Re: more cone6 ox glazes- EVERYBODY please!!!


> Patrick, there is not enough information here to know what
> glaze you would be talking about. Sometimes when people
> reply, the mail seems to form an automatic link to the
> previous pot, but you don't even have that.
>
> People, when responding to another post PLEASE provide
> enough information to make the link, otherwise it seems a
> waste. Perhaps the writer of the original message may make
> the connection, but if they are the only ones then send it
> directly to them and don't tie up the list. I came home from
> work tonight and had 96 messages to go through.
>
> patrick conrey wrote:
> >
> > Have you tried this glaze without the colorants???
> >
> >
____________________________________________________________________________
__
> > Send postings to clayart@lsv.ceramics.org
> >
> > You may look at the archives for the list or change your subscription
> > settings from http://www.ceramics.org/clayart/
> >
> > Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
> --
> Earl Brunner
> http://coyote.accessnv.com/bruec
> mailto:bruec@anv.net
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.