persimmon glaze test cone 6

updated sat 23 sep 00

 

NCGHandmadeTile@AOL.COM on fri 22 sep 00


Hi Alisa in Denmark,

Put your test back into the kiln and fire to 06, it turns from muddy brown
(kind of a honey amberish) to a mottled red. It is a really neat glaze. I
have seen it on bowls, I don't use it much on tiles, but we can get it to
work most of the time. If it is too thick it will blister.

Nancy G.