looking for cone 5-9 clay body recipes

updated mon 7 aug 00

 

Sarah Bailey on sat 5 aug 00


Hello all,

I'm trying to develop a good clay body to use for
low-relief tiles. The tiles will be fired in an
electric kiln between cone 5-9, so I'm looking for a
stoneware body that has a low warpage and low
shrinkage rate and is light-medium brown. If anyone
has any suggestions or recipes, I'd love to hear them.