search  current discussion  categories  glazes - misc 

good breaking glaze again

updated sun 6 aug 00

 

Wade Blocker on fri 4 aug 00


Michele,
Brush some of the original glaze over the crawled part and refire to
cone 6. I multifire. Your glazes should come outin perfect condition. Mia
in very hot ABQ

Michele on sat 5 aug 00


Thanks for all of the helpful responses!!! Sorry, I forgot to mention that
I fire to Cone 6 electric!! I will try floating blue as suggested and
transparent glazes over stains and oxide washes.

Thanks again,
Michele

P.S. My kiln DID underfire. It only reached 2079 F and the glazes have
crawled a bit as well as not matured. Can I just stick them back in and
refire to Cone 6? Will they smooth over? These are tried and true glazes
I have had no previous problems with! How accurate will the test tiles be
if I refire them?
Lots to learn!!