red burn out

updated mon 24 jul 00

 

Pancioli on sun 23 jul 00


In my experience with low fire reds, I found it best to fire them faster
than normal. They burn out more with slow firing.

Diana

Pancioli on sun 23 jul 00


In my experience with low fire reds, I found it best to fire them faster
than normal. They burn out more with slow firing.

It is also a good idea to apply them a little more thickly than usual.

Diana