Clayarters: here is the glaze I was looking for (only there are oxide =
colorants missing- Frank, can you supply them?)
This is a lovely satin emerald green glaze, good for terra cotta at 04, =
can be brushed on, dipped etc.
Sharon
-----Original Message-----
From: Frank Gaydos
To: sharon.miranda@oberlin.edu
Date: Wednesday, July 05, 2000 7:10 PM
Subject: Glaze


Sharon,
Sandy lives near me and here is the glaze:
Good Luck,
Frank

GBorate 31.54
Lithium Carb. 8.7
N.Synite 8.7
EPK 4.15
Flint 34.86
Whiting 16.6