sdpotter@GTE.NET on fri 7 jul 00


Greetings,
Did any one on Clay Art order 30 x 27 kiln
elements for positions 2 - 5 from Euclids about
3 months ago? Did you actually recieve a set for
a 23 x 27 positions 2 - 5?
I some how recieved the above while my kiln is the
smaller. Euclids told me to hang onto them until
further notice, but it's been almost 2 months. I
thought I would try and find the owner myself.
Euclids did send the correct size to me, at no charge.
Let me know off list... sdpotter@gte.net
Steve Dalton...the sun has finally peeked out 2 days in a row here in
Snohomish, WA