search  current discussion  categories  kilns & firing - gas 

cost of gas/lec

updated tue 4 jul 00

 

mel jacobson on mon 3 jul 00


it was only a few bucks.

itc maybe a hundred....quart of 100, pint of 296a, and a half cup
of 213.

burner was 20 bucks
coils, who knows what you have? maybe 50 bucks.
had the gas line, tank, etc.

had the spray stuff, but that is cheap.
it is a great idea by nils, a little common sense..and we
will see over the long haul how it works.

mel
money is no object if it works....think of taking a hulk, bringing
it back to life....fire bisque, cone 6 electric and cone 10 reduction
in the same kiln.
worth thousands.
of course, if you have a set of cone 6 glazes, why go to 10?
make your kiln a cone 6 reduction. great stuff there. no sense
changing all your horses....work with what you know.


FROM MINNETONKA, MINNESOTA, USA
http://www.pclink.com/melpots (website)