Sarah,
Laguna Clay company has cone 10 glazes. Many of their glazes are based on
Carlton Balls recipes.With a little testing the glazes work very well.
Laguna is located in the City of Industry in Southern California. They have
a website with all the pertinent information. Their phone is 800-452-4862.
Other clay companies carry their glazes, eg. Leslie Ceramics and Axner.
Axner carries only four of their cone 10 glazes. For the best glaze
selection I would call up Laguna's the web site, look under ceramic supply
companies. Mia in ABQ