Wade Blocker on thu 15 jun 00


----------
> From: Coolpots@AOL.COM
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Re: Beginner glaze question
> Date: Wednesday, June 14, 2000 6:58 PM
>
> I don't know what cone you are firing to but the Mason Stains shouldn't
be
> fired over cone 5. They can be fired lower also.
>
> Vicki
>
> That is not correct. Most Mason stains can be fired to cone 10 in
oxidation There are only a few that are fugitive.eg. pinks which fire only
to cone 02. Mia in ABQ