fwd: murrays borate analysis

updated fri 26 may 00

 

mel jacobson on thu 25 may 00


>From: Kickwheel@aol.com
>Date: Thu, 25 May 2000 10:56:43 EDT
>Subject: Murrays Borate analysis
>To: melpots@pclink.com
>X-Mailer: AOL for Macintosh sub 28
>
>Hi Mel,
>How have you been since Alabama, glad to see you are doing well. I enjoyed
>your banter and demonstration.
> Since you have our analysis up, would you mind pointing folks to our
>Murrays page because it gives usage information and photos of it. I think it
>is helpful for people to know a little more than a chemical breakdown,
>although that is useful. We are trying to be as helpful as possible.
> It is, of course, your call. The address is:
>http://kickwheel.com/Murrays.Borate.html
>Christine Winokur, President
>Kickwheel Pottery Supply



FROM MINNETONKA, MINNESOTA, USA
http://www.pclink.com/melpots (website)