Priscilla Wilson and/or Janice Lymburner on mon 22 may 00


Thanks to those who took the time to advise a novice about my plaster =
mold release problem!=20
=20
I'm going crazy trying to repair tiny bubbles in pieces cast with =
stoneware slip! It doesn't seem to matter how careful I am with mixing =
or if I try to get the bubbles to rise to the surface before I pour. I =
would really appreciate any suggestions.

Priscilla Wilson