Date: Fri, 5 May 2000 15:52:17 EDT
From: Veena Raghavan <75124.2520@compuserve.com>
Subject: Re: GOOD^6 GLAZE BOOK?-Lana Wilson

----------------------------Original message----------------------------

Message text written by Ceramic Arts Discussion List
>I will try to get our 10 best to you. One is a great Ohata Iron Red, a
celedon, a copper red, a "sexy" black matt. The bases glazes give soft
blue, pumpkin, gold, etc.
Marcia
<

Hi Marcia,
Can any of these glazes be used in Cone 6 oxidation? If so, I
would
really appreciate it, if you could include me in your post of your ten
best
glazes.
Thanks in advance.
Veena

Veena Raghavan
75124.2520@compuserve.com

Hi Marcia,

Me too please for the oxidation ones!

thanks,
Centa

Joanne L. Van Bezooyen on mon 8 may 00

Could Marcia share these with the clayart list, please.?

centa wrote:

> ----------------------------Original message----------------------------
> Date: Fri, 5 May 2000 15:52:17 EDT
> From: Veena Raghavan <75124.2520@compuserve.com>
> Subject: Re: GOOD^6 GLAZE BOOK?-Lana Wilson
>
> ----------------------------Original message----------------------------
>
> Message text written by Ceramic Arts Discussion List
> >I will try to get our 10 best to you. One is a great Ohata Iron Red, a
> celedon, a copper red, a "sexy" black matt. The bases glazes give soft
> blue, pumpkin, gold, etc.
> Marcia
> <
>
> Hi Marcia,
> Can any of these glazes be used in Cone 6 oxidation? If so, I
> would
> really appreciate it, if you could include me in your post of your ten
> best
> glazes.
> Thanks in advance.
> Veena
>
> Veena Raghavan
> 75124.2520@compuserve.com
>
> Hi Marcia,
>
> Me too please for the oxidation ones!
>
> thanks,
> Centa

Joanne L. Van Bezooyen on mon 8 may 00

Could Marcia share these with the clayart list, please.?

centa wrote:

> ----------------------------Original message----------------------------
> Date: Fri, 5 May 2000 15:52:17 EDT
> From: Veena Raghavan <75124.2520@compuserve.com>
> Subject: Re: GOOD^6 GLAZE BOOK?-Lana Wilson
>
> ----------------------------Original message----------------------------
>
> Message text written by Ceramic Arts Discussion List
> >I will try to get our 10 best to you. One is a great Ohata Iron Red, a
> celedon, a copper red, a "sexy" black matt. The bases glazes give soft
> blue, pumpkin, gold, etc.
> Marcia
> <
>
> Hi Marcia,
> Can any of these glazes be used in Cone 6 oxidation? If so, I
> would
> really appreciate it, if you could include me in your post of your ten
> best
> glazes.
> Thanks in advance.
> Veena
>
> Veena Raghavan
> 75124.2520@compuserve.com
>
> Hi Marcia,
>
> Me too please for the oxidation ones!
>
> thanks,