Diane G. Echlin on fri 5 may 00

Well Folks, my first ever studio show is tomorrow, and despite the fact
that my kiln went on the fritz last week I was able to do a final glaze
firing in another kiln. I opened it up this morning and was greeted
with the most stunning incarnation of Floating Blue I have ever seen.
So I set up my display with myriad teapots, mugs, and espresso cups,
sprinkled whole coffee beans around just for fun, and I'm ready to go.
I also had test tiles of a couple other glazes I got from clayart
members (thank you, Bacia!) that were exactly what I was looking for.
Gosh, I love pottery!