Cheryl L Litman on mon 3 apr 00

Here's the post everyone is still asking for from Lee Love on square
plates.

Cheryl Litman ---------- Somerset, NJ --------- email:
cheryllitman@juno.com

***Experience is what allows you to recognize a mistake......when you
make it again.***

--------- Forwarded message ----------
From: Lee Love
To: CLAYART@LSV.UKY.EDU
Date: Fri, 18 Feb 2000 11:13:46 EST
Subject: Re: square plates
Message-ID:

----------------------------Original message----------------------------
At the first pottery I working in, here in Mashiko (I worked there for
two
and a half months), the most interesting thing I learned was what they
taught all the new employees in the beginning: making plates, sushi
platters and pickle dishes just using a cutout, some newspaper and
extruded
clay coils (hebi nendo = clay snake.)

Most of the templates were cut out of light plywood and were either
squares
or rectangles or rounded cornered squares or rectangles, but you could
actually use any shape and cut them out of card board. The clay is
smoothed with a metal scraper on both sides. you then lay it on 3
sheets
of paper on a board,the paper is a little bigger than the slab you use
(we
cut the slabs from a block of clay, using a cutting wire and cutting
slats).
Lay the template down and cut the shape you want. Remove the excess
clay. Then, take come clay snake and put it under the edge of the clay
shape, so that half of the snake is covered by the edge of the slab.
On
square or rectangular shapes, you lay snakes at parallel ends, and then
you
lay the two other sides, with the ends crossing the first snakes. The
snakes should be under two sheets of paper, and on top of the bottom
sheet.
Next, take a cotton bag filled with cornstarch (tie the end with a rubber
band to hold the starch in) and smooth the slap from the middle to the
edge. To get a nice smooth surface on the wall of the outside of the
plate, lift the two pieces of paper and roll the cornstarch bag into the
edge, toward the clay snake. When you have all the edges the way you
want
them, slide the form off of the board with the paper and snakes intact
and
leave it out to dry. When it is dry, you can smooth the edges with a
shammie.

Where I work now, I am developing a new respect for molded work.
I work next to the retired Forman who makes most of the molded bottles,
jars, bowls, etc. Right now, he is making little calligraphy water
droppers. I think he does most of the production of these molded forms
and does the finishing, but the Sensei does the enamel work on them. I
want to learn the mold work so my wife can make her own work and do he
decoration on them. The slab work would also be nice flat surfaces
for
her to put her imagery on.

--
Lee in Mashiko, Japan