Can anyone tell me if it's possible to convert Ron Roy's ^ 6
oxidation Black recipe for use in ^ 10 reduction? I have a ^10
reduction black that's beautiful, but has way too much cobalt in it.
TIA.

C. A. Sanger
ShardRock Clay Studio
Kansas, USA
www.ikansas.com/~chuck/

ILENE MAHLER on sat 25 mar 00

If you are looking for a slightly matt black, write back and I willl be
glad to share it..It works teriffic on Lagunas' b-mix.. Ilene in Conn

"C. A. Sanger" wrote:
>
> ----------------------------Original message----------------------------
> Can anyone tell me if it's possible to convert Ron Roy's ^ 6
> oxidation Black recipe for use in ^ 10 reduction? I have a ^10
> reduction black that's beautiful, but has way too much cobalt in it.
> TIA.
>
> C. A. Sanger
> ShardRock Clay Studio
> Kansas, USA
> www.ikansas.com/~chuck/