search  current discussion  categories  kilns & firing - misc 

bourry fireboxes

updated mon 13 mar 00

 

iandol on sun 12 mar 00

-------------------
There are some plans for kilns which use Bourry fireboxes in Handbook for
Australian Potters, DeBoos, J.,Harrison, S., Smith, L. 1st Ed 1984. Methuen.
ISBN 0-454-00448-6 pp288, 291.

Hope that helps,

Ivor Lewis