search  current discussion  categories  kilns & firing - salt & soda 

amount of salt required to vapour glaze

updated mon 28 feb 00

 

The Smith's on sun 27 feb 00

-------------------
A short wile ago I posted a message asking if anyone could give me some
information about vapour glazing and I received a very helpful reply.... I =
the
interim I managed to locate a source for various metal and other =
salts.....Now I
need to ask an other question..... What are the amounts of salts required...
such as maximum and minimum amounts in order to see any results ??