search  current discussion  categories  techniques - terra sigillata 

terra sig tools

updated mon 14 feb 00

 

Cindy Strnad on sun 13 feb 00

------------------
To everyone who was interested in making Vince's terra sig . . .

The winemaker's siphon (called a racking cane) is available from Home Brew
Heaven http://www.homebrewheaven.com for 2.95, siphon tubing =40 .40/ft.

For those of you who missed the first exchange, the address for Vince's =
terra
sig instructions is:
http://digitalfire.com/education/glaze/terasig.htm


Cindy Strnad
earthenv=40gwtc.net
Earthen Vessels Pottery
RR 1, Box 51
Custer, SD 57730