search  current discussion  categories  kilns & firing - misc 

sv: re: kiln report--firing speed question

updated tue 25 jan 00

 

Alisa and Claus Clausen on mon 24 jan 00

------------------
Hi Tim,
Blah, I just bought orton cones and can not find the following info. in my
catalog.
I forgot how to place them in the kiln pack.

Which way should the pressed in cone number face? For example, I have three
cones in the pack all tilting a bit forward, and the cone mark it facing
forward. Is this correct. I do not want them to melt doing backdives=21

Thank you
Alisa in Denmark