search  current discussion  categories  glazes - specific colors 

yellow stain

updated tue 11 jan 00

 

Gary Kelsey on mon 10 jan 00

-------------------
Tom,
I see that Mason stains 6433 =26 6450 contain praseodymium, about what =
percent
of stain should be added to the base glaze?
Do you have any suggestions for the base glaze? I always learn something =
from
glaze test, but trial and error is a long process.
Thanks,
Gary