search  current discussion  categories  glazes - specific colors 

hunt for good red glaze

updated thu 2 dec 99

 

CAROLYN GEORGE on wed 1 dec 99

Hi, Chris, accept my apology please.. I responded to the wrong glaze
recipe.. Yes, it was the Shiny Red to Purple Kemp 17 glaze.. I fired to
^5 and to ^ 6.. both with the same results... glaze fit wonderful, just
a washed out pink. no purple also tried Desert Buff clay with it as
well, same result..I haven't had the time to test the original glaze you
posted, but will right after my next 2 upcomings shows.. Thanks and hope
I didn't confuse the issue...carolyn in now REALLY cold Carolina