Sara Gilstrap on tue 23 nov 99

Below you will find two different reds at Cone 6.

Shiny:
Gerstley Borate 210
Neph Syenite 160
EPK 110
Whiting 200
Flint 220
Tin ox 45
Chrome Ox 1.35

Cranberry Matte:
Barium Carb 38.4
Lithium Carb 2.06
Zinc Ox 15.11
Custer Feldspar 31.07
Flint 13.36
Nickel Carb 4
Gerstley Borate .7 Please experiment with the Gerstley. Too dry without it.

---------------------------------