search  current discussion  categories  glazes - specific colors 

cerdec-yellow inclusion stain

updated mon 8 nov 99

 

Hank Ray on sun 7 nov 99

Hey All

Thought i should report that if have done a test using Cerdec's yellow
inclusion stain, at cone 10 reduction.... this is a pricey stain.. at 40
bucks (usa) for a pound. i included it in the glaze base at 8 percent,
giving me about 2 and 1/2 gallons of glaze for a the 40 bucks... actually i
have just a little bitty bit left......

it is very yellow... on a white clay (b-mix) and a bright mustard on a very
dark clay (amador by laguna).... bet you could get away with less stain......

pete, over and out...

in OKC OK... USA