Alisa and Claus Clausen on sun 10 oct 99

------------------
The ceramic supplier in Denmark has received and read all the relevant =
postings
about the lime problems in bodies from Potclays. He has had problems with =
the
clays for a long time, but Potclays has never admitted to him that there is =
a
definite lime problem. It seems Janet was correct in her theory, that =
Potclays
was knowingly sending their contaminated clays to buyers outside the UK. =
The
supplier is very interested in highly motivated to get to the bottom of the
problem with Potclays. I am very satisfied with all the help I have =
received
from Clayart, and it seems that we have =22made a positive difference=22 =
today with
our input. Thank you all very much.

The supplier has sent me different samples to test in leiu of bodies I have =
been
using from Potclays. Otherwise, I am going to mix up two receipes I =
received
from Tom B. slurry and hang method, and get to work again.

I am signing off for 10 days from Oct. 13, when I go to New York. Books, =
books,
and more books.

Alisa in Denmark