Mary Ella Yamashita on sat 18 sep 99

Realized my original message was somewhat unclear. The cat jar was
originally ^6 fired with the Shoyu Brown glaze. I am considering painting
a lowfire clear glaze over the mason stained knob and refiring the piece at
^06. Will the refiring have an adverse affect on the ^6 Shoyu Brown glaze?