search  current discussion  categories  kilns & firing - cones & controllers 

oxyprobe in salt.

updated thu 26 aug 99

 

mel jacobson on wed 25 aug 99

i have not used mine in salt.
it is too valuable a tool for our
use to let it get corrupted in salt.

some others may have used it in this
application.
i would not.
mel/mn
http://www.pclink.com/melpots