Tony Hansen on fri 20 aug 99

We just got another cone 10R kiln load out with the last
production test of Ravenscrag Slip and it is even better.
It is melting to a glossy clear glaze when used 100%.
All the new multilayering tests worked very well.
If you want a sample, please visit the materials web
page at http://ceramicsearch.com/plainsman/data/raven.htm
Samples are free in Canada and $2 in the USA. This stuff
is really incredible, it will give students a chance to
create great glazes with high likelihood of success. I
can't remember ever being as excited about a material
as I am about this stuff.

--
Tony Hansen, Plainsman Clays Ltd.