Hello Pamala, you should get a pretty strong result with 3% additions of
Cerdec stains in your glazes, fired to 1160C or thereabouts - higher temps
are up to you. Lower percentages give good results too, and the stains can be
mixed to achieve other colours - only beware zinc in your formulae for some
colours.