Reposting on wood powder clay:

>Just want to add that I am skipping the paper part of the process and using
>wood powder that gets cleaned out of the sanders at the woodshop down the
>road. It takes me afew minutes to pour parts out onto a big tray to grab
>out the bits of this and that and into the already-blended slop it goes.
>It makes GREAT paperclay. And I love that all the refining that goes into
>making paper isn't going into the clay just to be burned out.
>
>Eleanora
................