sv: re: sv: re: clear glaze crazing.

updated mon 2 aug 99

 

Alisa and Claus Clausen on sun 1 aug 99

------------------
Thanks a lot Dave for your reply.

Right, that the crazing only appears on work fired to 04.
Unfortunately up until now I have been using a communal studio where all the
glazes are commercial.
I have since these postings called the supplier, and they recommended =
another
transparent for 04 that they
swear (yup) does not craze on the =22wide range=22 white body I am using.

Now, I have just moved into my very own studio just built on our property. =
I
=22inherited=22 an absolute landfall of raw materials. I am just sorting =
through it
all and will of course want to mix my own glazes. I am awaiting the arrival=
of
my new old electric kiln next week. Once I come into production, I would =
like
to exchange ideas about transparents for 04 and 6.

Hope you had a good weekend,
Regards,