Hey there...

you can get great greens at cone 6 oxidation.,.....

use any good clear you have and add Copper oxide of different amounts.... do
some testing...at cone 6 ox copper oxide can do some fun things... because it
will mottle and do different effects not possible at cone 10 or cone 6 with
copper carb... just an idea