Des Howard on tue 6 jul 99

Ahmad
"Monoporosa" & "Monocottura" are once-fired tile products of the of the
heavy clay industry. A quick look via www.altavista.com shows 63
references. I think that would be more productive of answers than Clayart.
Best of luck
Des Howard

Ahmad Mokhtarifard wrote:

> ----------------------------Original message----------------------------
> I need some information regarding "monoporosa"
> and "protecting glaze."
> This is for my friend that is in a severe need of
> information. He is investing on clay and ceramics.
> Thanks a lot.
>
> Yours sincerely,
> Ahmad Mokhtarifard
> mokhtara@sums.ac.ir