search  current discussion  categories  glazes - specific colors 

glaze mistake, emily's purple

updated tue 6 jul 99

 

Lesley Alexander on mon 5 jul 99

To Nancy, You don't LIKE the lighter purple frosting? To me that's what
makes it so absolutely lush. I've only fired it twice, but both times have
gotten a purple with a slightly lighter purple blush. However, if
blue/purple is what you usually get....maybe that's the norm and your
current batch and I are both off??? You could do a line test to see what
happened. Good luck. Lesley in So. Calif., send us some of your rain.