Just from my limited experience---I made up batches of the outdoor clay body
for Cone 6 from the Val Cushing handbook. I probably have used about 600
pounds of this clay. It is formulated to withstand cold temperatures and fires
to Cone 6. I found it easy to work with and really liked it. It looks good in
oxidation---has a warm light brown color.