=3EFrom what D.Creber writes, I can anticipate only the following problem: =
cone
=3E6 is not at least 400oF (222oC) above the crystal growth temperature =
window,
=3Ethe minimum top temperature she suggests for macrocrystalline glazes =
proper
=3Edevelopment.

I just realized that she meant 400oF above the melting point of the glaze
which does not constitute a problem.