cone 6 porcelain.

updated fri 21 may 99


susanford on thu 20 may 99

Has anyone used any formulated for cone 6 pocelain? I am
getting an elecric kiln soon, and I'll be moving my work
from cone 10 reduction to cone 6 oxidation. I want to be
able to continue some work with porcelain, and I've noticed
some adds here and there for it.

Any comments? How's it handle? How does it compare to
high fire porcelain? Any suggestions would be welcome.

Susan K. Ford