Carol Tague on sat 1 may 99

Hi Laura, Florida Clay Art Co. in Sanford FL sells US Pigment Stains. You
can get a free catalog. 1-800-211-7713


>----------------------------Original message----------------------------
>Hi Everybody!!
>
>I am looking for a source for the following stain manufacturers:
>
>Drakenfeld
>Standard
>O'Hommel
>US Pigments
>
>Does anyone know where I can buy these? I live in south Florida...
>...where summer is here already