Paul Lewing on fri 14 may 99

I recently picked up an overglaze felt tip pen made by Potteycraft in
Stoke-on Trent, England. When I tried using it, I couldn't get anything
to come out. The felt tip was originally dry and clean, and after
fiddling with it for a while, I did get some solvent to come out, but no
color. Is there a trick to using these gizmos, or do I just have an old
or defective one? It seemed like such a good idea, I just hope it will
work.