search  current discussion  categories  kilns & firing - construction 

kiln repair and first fire, empty or not?

updated fri 14 may 99

 

Chuck Nunnelly on tue 11 may 99

I used some kiln cement to repair some brick damage in my electric kiln. The
maintenance tells me to fire it to cone 5 empty the first time. I have a
load ready to glaze fire to cone 6 and wonder what risk I take by skipping
the empty fire and going ahead with the glaze fire.

Chuck Nunnelly
Mechanicsville VA

Don & Isao Morrill on thu 13 may 99

At 11:42 5/11/99 EDT, you wrote:
>----------------------------Original message----------------------------
>I used some kiln cement to repair some brick damage in my electric kiln. The
>maintenance tells me to fire it to cone 5 empty the first time. I have a
>load ready to glaze fire to cone 6 and wonder what risk I take by skipping
>the empty fire and going ahead with the glaze fire.
>
>Chuck Nunnelly
>Mechanicsville VA
>

Chuck, We have first-firedboth empty and filled. Slowly does the trick.
The only problem we recognize is the possible effect constituents of the
cement might have on the ware. We have had no problem with htis but it
might be well to be aware. You do not mention the WXTWNT of the repairs.
ISao & Don