search  current discussion  categories  glazes - specific colors 

blue-green glaze

updated thu 6 may 99

 

Frank Simons on wed 5 may 99

Hi to you all--
Does anyone remember or maybe filed a post of a few months back giving the
recipe for a cone 6 ox. blue-green?greenblue? glaze that the poster used on =
her
christmas ornaments? I have searched the archives with negative results. I =
had a
nice blue-green rutile glaze that I dearly loved, but after replentishing my
supply of rutile, my beautiful jade green glaze suddenly turned into a
donkey-poo brown which all amounts of adjusting have failed to rectify. I =
would
be eternally greatfull for anyone wishing to share a =5E6 blue-green either=
by
post or direct email.

Thanx Frank Simons, Penticton, B.C. fsimons=40img.net