ron roy is a genius!

updated sat 24 apr 99

 

L.P. Skeen on fri 23 apr 99

Yahoo! Just opened the kiln and pulled out 2 different "Ron Roy
Variation" tests. I made Floating Blue #1 and a revision of a barium
fritted shino and the new glazes are DEAD RINGERS for the original
recipes. Hot diggety, thanks Ron!
--
Lisa Skeen ICQ# 15554910
Living Tree Pottery & Soaps http://www.uncg.edu/~lpskeen
FAILURE IS NOT AN OPTION!!! It comes bundled with the software.