glaze colors

updated sun 25 apr 99

 

Marty Anderson on fri 23 apr 99

Hello everyone,


Frank Gaydos has graciously loaned my pots space on his web site for a week =
so
everyone can see the colors. It became impossible for me to answer all the
email I received about the glazes. If you want the recipes for the glazes I
have not already posted, email me direct and I will send them to you. I =
hope
the pics do a good enough job showing what the colors look like. The base =
color
is what is stated, but each pot has up to 9 other colors sponged randomly on
them.

All are fired =5E6 oxidation. No special firing. Set my computer to =5E6,=
medium
and go off and leave it til it's done. It is not unusual for me to lift the=
lid
to take a peek anywhere from 200-500 degrees. No soaks at the end. The red=
is
always red and is applied VERY thick. 95=25 of my pots are grogless medium
tan/brown spotted clay.

If I have not answered all the questions emailed to me, please send me =
another
email and I will answer as soon as possible.

Vince, I used the spell checker so if anything is wrong, the computer did =
the
deed.

www.erols.com/fgaydos/Slides.html


marty
martya=40airmail.net

ababy sharon on sat 24 apr 99

Hi! THis morning when I took my dauther to the Kibbutz`s dining room(from
there Goes the school bus) I told her about Jo`s glaze as she is the only
one in my family that would be shocked from the amount of Iron(or any thing
at all) I mant to try this glaze! I have seen the nice works-with the nice
glazes at Frank Gaydos`s site.I thinnk it is very nice of him
to have does chaging guest-works at his site!
I would like to get from you the recipes of the others glazes.As for me I
made a lote of testings latly after repeating on them with more then the
100gram -if they will work well I `ll send them thrugh CLAYART.
Thanks
Ababi-----Original Message-----
From: Marty Anderson
To: CLAYART@LSV.UKY.EDU
Date: Friday, April 23, 1999 05:18
Subject: glaze colors


----------------------------Original message----------------------------
Hello everyone,


Frank Gaydos has graciously loaned my pots space on his web site for a week
so
everyone can see the colors. It became impossible for me to answer all the
email I received about the glazes. If you want the recipes for the glazes I
have not already posted, email me direct and I will send them to you. I
hope
the pics do a good enough job showing what the colors look like. The base
color
is what is stated, but each pot has up to 9 other colors sponged randomly on
them.

All are fired ^6 oxidation. No special firing. Set my computer to ^6,
medium
and go off and leave it til it's done. It is not unusual for me to lift the
lid
to take a peek anywhere from 200-500 degrees. No soaks at the end. The red
is
always red and is applied VERY thick. 95% of my pots are grogless medium
tan/brown spotted clay.

If I have not answered all the questions emailed to me, please send me
another
email and I will answer as soon as possible.

Vince, I used the spell checker so if anything is wrong, the computer did
the
deed.

www.erols.com/fgaydos/Slides.html


marty