search  current discussion  categories  kilns & firing - raku 

re-to justin--raku burgandy matte

updated tue 13 apr 99

 

Pamala Browne on mon 12 apr 99

I tried to get to you via hotmail but no luck.Here is the recipe and the =
site
where it was found --lots of stuff to try there--check it out.I don't know =
how
to format yet so it comes out straight.sorry.DRY BURGANDY MATTE
COLEMENITE 50=25 TALC 30=25 NEPH SY 20=25 ADD =
COPPER
CARB 3=25 This is my current fav glaze--have fun=21The site =
where
obtained is www.utpb.edu/artsci/art/ceramics/glazes/raku.htm