search  current discussion  categories  people 

lana wilson glazes

updated fri 5 mar 99

 

Barbara Lewis on thu 4 mar 99

I've tried Lana's Bronze Aqua. It is a very nice glaze that is bronze where
thick and aqua where thin. I've also tried Bell's Lichen, Tom West and
Persimmon glazes. It's true that Tom West and Persimmon when fired once to
cone 6 will be brown but when refired will look like a reduction iron red.
These glazes where handed out at by Lana at the 1993 NCECA Conference in San
Diego. Barbara

At 09:14 AM 3/3/99 EST, you wrote:
>----------------------------Original message----------------------------
>Has anyone tried any of the glazes Lana has offered in her sprial notebook
>which she sells by mail? I am particulary interested in her turquoise glazes.
>Thanks in advance.
>
Wellspring Clayworks
5412 Well Spring Road
La Plata, MD 20646
blewis@crosslink.net