Chris Schafale on fri 26 feb 99

Oops, I forgot to mention that Ron requested that anyone who tries
these recipes please post the results to the list, so we will get
more feedback on how they work. Thanks!

Chris
Light One Candle Pottery
Fuquay-Varina, NC
candle@nuteknet.com

Veena Raghavan on sun 28 feb 99

Chris and Ron,
I am in the process of testing #2. I have only tested very small
pieces so far, but it seems to be working out very well. Want to make up a
larger batch, and try it on a larger piece. I have brushed it on, due to
the small quantity, and got a nice glossy black. Will post more as I test
larger. This was on Cone 6 stoneware.
All the best.
Veena
Veena Raghavan