Brian Crocker on fri 5 feb 99

G'day Earl,

I dont know who the person is that asked about the drying crack problem but
is it worth passing on? I have several different sizes of octagonal 3mm
glass which I
place on the rim of platters and bowls, it keeps the rims horizontal, [
ie.,not wavey ] and controls the drying. Cant remember when I had the last
problem.

Kind regards, Brian C.,