search  current discussion  categories  glazes - misc 

unity molecular formulae

updated sun 24 jan 99

 

Brian Crocker on thu 21 jan 99

Dear CLAYARTERS,
Does ony one have " Unity Molecular Formulae " for Ferro Frits and for that
matter any other Frits, I'm trying to gather a wide reaching chart hopefully
of all Frits
so that when each one of us sends out a Formula with a Frit or two in it the
reciever can hopefully look up the chart and then know what local Frit will
fit in.

This may take some time but I hope it will bring communication together.

Kind regards to all Brian C.,
Brian Crocker
Tea Tree Gully, South Australia,
{e.mail} crocker@dove.com.au

"Never loose sight of the bigger picture,"
"Never loose sight of what you set out to achieve."
NAB.

Dale Mark on sat 23 jan 99

Hello Brian

Check out "Frit Formulas" by William Hunt, Ceramics Monthly May 1978
pp.48-54.

Dale Mark
Hamilton, Ont.