GARY GREENBERG on fri 25 sep 98

I have been firing wet ware in Weber grills, brick pits, gas and electric
kilns utilising aluminum foil to facilitate the formation of the steam
blanket since 1989 and have conducted numerous workshops on the process.
For more information see:

NCECA Journal, Vol. 12, 1991-92
FOIL FIRING "From Pugmill to Gallery in Three to Five Hours" pp.54-56

Ceramics Monthly, Feb. 1992
FIRING WET POTS pp. 80-82

If you cant find the articles e-mail me with your mailing address and
I'll send you copies.