I find that the basic raku glaze of 80% gerstley borate / 20% nepheline
syenite with up to 15% zircopax (or alternatively 5% tin oxide) is off
white on Armadillo Clay's Balcones. This clay is a light peach-tan when
bisqued. Is there anything to try to get a more pure white glaze on this
clay or do I need to use a white clay body? If so, how much sand or grog
should I add to their Dillo White or porcelain to get a throwable clay that
will withstand raku?

Also, as a newbie, I've learned a lot from this group but haven't given
anything back up to now. Here's a start. I've collected about 100 raku
glaze recipes from various sources and stored them in GlazeChem, a
shareware program. If you would like a copy of the GlazeChem data file
(about 75kb), send me email. The file is designed to be used by GlazeChem,
but can be read using a text editor as well.

deg

Wilkinson on tue 10 nov 98




----------------------------Original message----------------------------
I find that the basic raku glaze of 80% gerstley borate / 20% nepheline
syenite with up to 15% zircopax (or alternatively 5% tin oxide) is off
white on Armadillo Clay's Balcones. This clay is a light peach-tan when
bisqued. Is there anything to try to get a more pure white glaze on this
clay or do I need to use a white clay body? If so, how much sand or grog
should I add to their Dillo White or porcelain to get a throwable clay that
will withstand raku?
.....................

I use Dillo White just as it comes from the bag for raku and it works
beautifully.

Lori Wilkinson
LorWilk@dfn.com
http://www.geocities.com/SoHo/Gallery/1165

Quentin D Maxwell on tue 10 nov 98

On Mon, 9 Nov 1998, Dewitt Gimblet wrote:

> ----------------------------Original message----------------------------
> I find that the basic raku glaze of 80% gerstley borate / 20% nepheline
> syenite with up to 15% zircopax (or alternatively 5% tin oxide) is off
> white on Armadillo Clay's Balcones. This clay is a light peach-tan when
> bisqued. Is there anything to try to get a more pure white glaze on this
> clay or do I need to use a white clay body? If so, how much sand or grog
> should I add to their Dillo White or porcelain to get a throwable clay that
> will withstand raku?

I don't know about Dillo White or porcelain, but I use a basic
02-04 white clay from L&R Specialties in Nixa, Missouri and mix 10% fine
white sand or fire brick grog. I make sure I get a good 04 bisque too.
Hope this helps!

Peace & Prayers,
Q.
qmaxwell@mail.llion.org

Khaimraj Seepersad on wed 11 nov 98

Tried to e-mail you , system says your address has a problem ,please contact me

-----Original Message-----
From: Dewitt Gimblet [SMTP:dewitt@bga.com]
Sent: Monday, November 09, 1998 10:26 AM
To: CLAYART@LSV.UKY.EDU
Subject: Trying for a good white crackle raku glaze

----------------------------Original message----------------------------
I find that the basic raku glaze of 80% gerstley borate / 20% nepheline
syenite with up to 15% zircopax (or alternatively 5% tin oxide) is off
white on Armadillo Clay's Balcones. This clay is a light peach-tan when
bisqued. Is there anything to try to get a more pure white glaze on this
clay or do I need to use a white clay body? If so, how much sand or grog
should I add to their Dillo White or porcelain to get a throwable clay that
will withstand raku?

Also, as a newbie, I've learned a lot from this group but haven't given
anything back up to now. Here's a start. I've collected about 100 raku
glaze recipes from various sources and stored them in GlazeChem, a
shareware program. If you would like a copy of the GlazeChem data file
(about 75kb), send me email. The file is designed to be used by GlazeChem,
but can be read using a text editor as well.

deg